Acrylic Thickener
Product Name : Acrylic Thickener
Color : Off – White Organoclay Powder
Application: Thixotropic Uses Paints | Coatings | Grease | Oil drilling Mud
Materials : Alkyl Quaternary Ammonium bentonite
Certificate: ISO 9001
Packing: 25Kg/Bag,22.68 (50lb)/Bag Or Customize
16MT/20FCL With Pallet, 22MT/40FCL With Pallet.
Features : Thixotropy, Thickening, Anti-Settling, Anti-Sagging,
Sample Service : Acrylic Thickener Sample Available.
Brand : Camp – Shinning Organoclay
Acrylic Thickener
Acrylic Thickener also named paint thickening agent and organoclay rheology modifier.Acrylic thickener has good thixotropy and thickening. Rheologieadditive could assist paint and pigment manufacturers to produce stabilized emulsions and anti settling solutions.
Anti settling agent also named paint thickening agent and thixotropic agent for epoxy (common name Organoclay ).
In paint industry, organoclay could use for solvent based paint and water based paint.
Rheologieadditive is adapted for aromatic solvent, ester, ketone, alcohol and resins in medium and high polarity such as two-component polyurethane, fluorocarbon coating, epoxy coating, zinc-rich coating etc.
Organoclay bentonite CAS :68953 – 58 -2
Sale Dept: [email protected]
Cell(Whatsapp): +86-13185071071
How To Use Thixotropic clay
- Pre-gel method
- Polar activator is not necessary:
- Main solvent xylene: 95~92%
- Thixotropic clay :5~8%
- Dispersing 5-15min, gel is finished.
- Polar activator is necessary:
- In aromatic solvent, the recommend activator is methyl acohol/water (95%/5%)/ acolhol/water (95%/5%), the dosage is 33%-45% based on the weight of CP-720B.
- In mineral oil (such as 200#), white oil, diesel oil, the recommend activator is methyl acohol/water (95%/5%)/acolhol/water(95%/5%), the dosage is 33%-60% based on the weight of CP-720B.
- Procedure of adding gel:
- Charge solvent and resin to mill
- Slowly add the gel
- Dispersing 5-10min
- Wetting agent (if required)
- Disperse completely to desired fineness
- Dilute to desired viscosity
- Add directly with powder
- Charge solvent and resin
- Add Thixotropic clay slowly
- Disperse 10-15min
D .Add polar activator (if necessary)
- Disperse 10-15min at high speed
- Add wetting agent and other additive
- G.Grind and next procedure
It can be added directly in powder under high shear condition. The addition is recommended to be before grinding procedure to get the best effectiveness. Addition level is commonly 0.1%~2.0%. If add polar activator and make pre-gel, better efficiency can be achieved.
Acrylic Thickener