innerpagebg

Application

Send Enquiry

  • Organoclay Rheology additive with high gelling efficiency,light color gel and produce reproducible thixotropic consistency over a wide temperature range
  • Imparts particle suspension, preventing hard settling of pigment and fillers.
  • Exerts strong film reinforcing action in organic binder systems.

Organoclay Rheology additive is used in marine paint, Industrial paint, heavy-duty, anticorrosion paint such as bituminous coatings, polyester paints, Alkyd paints.

Organoclay Rheology additive also is used in Sealant,Inks,grease and unsaturated polyester putty.

Safety

All safety information is provided in the Material Safety Data Sheets for Zhejiang Camp-Shinning New Material Co.,Ltd..

 

Package

Kraft paper bag with PE liner or multi-wall paper sacks or customized. 25kg/bag or 22.68kg/bag or customized

 

Storage

CP-34 has a shelf life of 2 years, and should be stored in ventilated cool and dry place.

 

Notice

The information on use is based on data which are believed reliable, but any recommendation or suggestion made is without guarantee or warranty, since the conditions of use are outside our control. All products are sold on the conditions that purchasers shall make their own tests to determine the suitability of such products for their purpose and that all risks are assumed by user. We disclaim any responsibility for damages resulting from careless or improper handling or use. Nothing herein is to be taken as permission, inducement or recommendation to practice any patented invention without a license.

Using

Organoclay Rheology additive disperses under high shear and requires a polar activator for best efficiency. Heat is not required to obtain good dispersion. Addition levels are typically in 0.2%~2.0%. Polar activator (95% Ethanol or 95% Methanol) is needed. Normally addition level of polar activator is recommended to be 40%~50% of CP-34 in weight. If in xylene system, addition level of polar activator is about 30%-40% of CP-34 in weight.

Pre-gel is made as below procedure.

  1. Charge solvent to mill
  2. Slowly add CP-34(6-10% by weight of total pregel) to mill under agitation.
  3. Mix at high speed for 5 minutes.
  4. Add polar activator.
  5. Mix at high speed for 5 minutes.
  • We are looking for distrubitor in the world. If you are interesting our Organoclay Rheology additive,pls mail us:
  •  [email protected]
  • Mob: 0086-131 85 071 071

Send Enquiry

//